Aerocom Tech Centre

72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe, Annealed
BackThis specification covers a corrosion and heat resistant nickel alloy in the form of sheet, strip, and
plate.
Property | Min Value | Max Value |
N/mmsq 0.2% Yield Strength | 0 | 448 |
N/mmsq Ultimate Tensile Strength | 0 | 965 |
% Elongation | 40 | 0 |
% Reduction of Area | 0 | 0 |
Hardness Rockwell B (HRB) | 0 | 0 |
Hardness Rockwell C (HRC) | 30 | 0 |
Hardness Brinell (BHN) | 0 | 0 |
Hardness Vickers (HV) | 0 | 0 |
% Carbon (C) | 0 | 0.08 |
% Chromium (Cr) | 14.00 | 17.00 |
% Manganese (Mn) | 0 | 1.00 |
% Molybdenum (Mo) | 0 | 0 |
% Nickel (Ni) | 70.00 | 0 |
% Phosphorus (P) | 0 | 0 |
% Sulphur (S) | 0 | 0.01 |
% Silicon (Si) | 0 | 0.50 |
% Iron (Fe) | 5.00 | 9.00 |
% Copper | 0 | 0.50 |
% Magnesium | 0 | 0 |
% Zinc | 0 | 0 |
% Titanium | 2.25 | 2.75 |
% Aluminium | 0.40 | 1.00 |
% Cobalt (Co) | 0 | 1.00 |
% Zirconium (Zr) | 0 | 0 |
% Boron (B) | 0 | 0 |
% Lead (Pb) | 0 | 0 |
% Bismuth (Bi) | 0 | 0 |
% Selenium (Se) | 0 | 0 |