Aerocom Tech Centre

18Cr - 10.5Ni - 0.40Ti (SAE 30321), Thin Wall, Solution Heat Treated
BackThis specification covers a corrosion and heat-resistant steel in the form of welded tubing.
Property | Min Value | Max Value |
N/mmsq 0.2% Yield Strength | 241 | 0 |
N/mmsq Ultimate Tensile Strength | 517 | 724 |
% Elongation | 40 | 0 |
% Reduction of Area | 0 | 0 |
Hardness Rockwell B (HRB) | 0 | 0 |
Hardness Rockwell C (HRC) | 0 | 0 |
Hardness Brinell (BHN) | 0 | 0 |
Hardness Vickers (HV) | 0 | 0 |
% Carbon (C) | 0 | 0.08 |
% Chromium (Cr) | 17.00 | 19.00 |
% Manganese (Mn) | 0 | 2.00 |
% Molybdenum (Mo) | 0 | 0.75 |
% Nickel (Ni) | 9.00 | 12.00 |
% Phosphorus (P) | 0 | 0.040 |
% Sulphur (S) | 0 | 0.030 |
% Silicon (Si) | 0.40 | 1.00 |
% Iron (Fe) | 73.6 | 63.55 |
% Copper | 0 | 0.75 |
% Magnesium | 0 | 0 |
% Zinc | 0 | 0 |
% Titanium | 0 | 0.70 |
% Aluminium | 0 | 0 |
% Cobalt (Co) | 0 | 0 |
% Zirconium (Zr) | 0 | 0 |
% Boron (B) | 0 | 0 |
% Lead (Pb) | 0 | 0 |
% Bismuth (Bi) | 0 | 0 |
% Selenium (Se) | 0 | 0 |