- UNS Number - UNS A93003
- Specification - AMS-QQ-A-225/2
- Form - Bar, Rod, and Wire, Rolled, Drawn, or Cold Finished
General Information
This specification covers the specific requirements for 3003 aluminum alloy bar, rod, and wire produced by rolling, drawing, or cold finishing.
Mechanical Properties
Property |
Min Value |
Max Value |
N/mmsq 0.2% Yield Strength |
0 |
0 |
N/mmsq Ultimate Tensile Strength |
0 |
131.005 |
% Elongation |
25 |
0 |
% Reduction of Area |
0 |
0 |
Hardness Rockwell B (HRB) |
0 |
0 |
Hardness Rockwell C (HRC) |
0 |
0 |
Hardness Brinell (BHN) |
0 |
0 |
Hardness Vickers (HV) |
0 |
0 |
Chemical Elements
% Carbon (C) |
0 |
0 |
% Chromium (Cr) |
0 |
0 |
% Manganese (Mn) |
1.0 |
1.5 |
% Molybdenum (Mo) |
0 |
0 |
% Nickel (Ni) |
0 |
0 |
% Phosphorus (P) |
0 |
0 |
% Sulphur (S) |
0 |
0 |
% Silicon (Si) |
0 |
0.6 |
% Iron (Fe) |
0 |
0.7 |
% Copper |
0.05 |
0.2 |
% Magnesium |
0 |
0 |
% Zinc |
0 |
0.1 |
% Titanium |
0 |
0 |
% Aluminium |
96.7 |
98.95 |
% Cobalt (Co) |
0 |
0 |
% Zirconium (Zr) |
0 |
0 |
% Boron (B) |
0 |
0 |
% Lead (Pb) |
0 |
0 |
% Bismuth (Bi) |
0 |
0 |
% Selenium (Se) |
0 |
0 |